Re: Welding/fabrication thread.
Try lower your amps a bit. Seems like u have plenty of heat there. Also make sure you let the argon run for about 10 seconds at the end of your runs. This will prevent that pitting u see in some of your first ones at the end . Also try feather off the pedal as you heat that metal up especially near the ends. Welds look way better then when I first started so u are off to a great start in my opinion.
|